How to Make a Three Claw Wave Ring
- Description
The video shows you how to make a three claw setting using basic tools. It is then mounted on a wave shaped shank. This resulting project is demonstrated with a rare fire opal.
There are so many options that you could apply to this design to make it even more special.
Lessons Include:
- Part 1 - Three claw ring (Part one) - 52 min 59 sec
- Part 2 - Three claw wave ring (Part two) - 11 min 42 sec
Materials:
- 5mm round faceted stone (larger can be used)
- Sterling silver strip 0.7mm x 3.3mm x 40mm
- Round wire 1mm x 80mm & 1.5mm x 70mm
- Author
You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.