Rose Bezel Ring
- Description
This course demonstrates how to make a double bezel setting to look like a rose flower design. You will be shown some alternative manufacture methods that do not involve expensive machines and equipment.
This lesson includes three videos:
- Part 1 - Rose bezel ring - 49 min 50 sec
- Part 2 - Rose bezel ring setting - 14 min 57 sec
Materials:
- 5.75mm cubic zirconia
- Sterling silver: 1.2mm x 5.2mm x 45mm
- Sterling silver: 3.3mm x 3.3mm x 43mm
- Author
You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.