How to Make Graduated Byzantine Chain
- Length26 min 1 sec
- Description
This course will demonstrate how to make an impressive byzantine chain with graduated jump ring sizes to give it a tapered look. The linkage appears to be complicated but it's easier than it looks.
Materials:
- Sterling silver
- 7mm mandrel 1.5mm round wire x 14 jump rings
- 6mm mandrel 1.35mm round wire x 24 jump rings
- 5mm mandrel 1.2mm round wire x 24 jump rings
- 4mm mandrel 1mm round wire x 36 jump rings
- Sterling silver round wire 1.5mm x 40mm
- Author
You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.