How to Harden and Temper Tool Steel
- Length13 minutes 37 seconds
- Description
Learn to harden and temper your own custom-shaped jewelry tools. By master goldsmith Charles Lewton-Brain. Filmed in full HD 1080p.
IMPORTANT NOTE: Hardening and Tempering is a two step process, the steel MUST be tempered (softened) after hardening to be safe. Full details shown in the full version of the video.
- Includes
Purchase also includes these instructional PDF downloads:
- HardeningTempering.pdf
- GrindingWheelSafety.pdf
- Author
You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.