Article
How to Make an Agate Imitation Cabochon

This technique consists of the successive application of silver foil sheets, changing the colors of enamels among them, and then to wear away sectors, and discover each one of the colors used in the different layers. Apply the first of the layers…

Article
How to Work Enamel Hot

Photo 1: Apply a coat of enamel on a piece of domed copper and fire. Photo 2. A sheet of silver foil is adhered to the enamel surface with gum solution and fired. Photo 3: Once the foil has been fired, it is burnished with a glass brush. Photo 4:……

Article
Metallic Scratched Technique

This article describes how to do a metallic scratched technique in enamel designs in visual step by step procedure. ¬†Metallic Scratched Technique Apply the industrial liquid enamel by pouring and rotating Once the surface has been covered,…