How to Make a Thick Bezel Setting for a Stone Cabochon
- Description
This video will guide you through the process of making a thick bezel setting for a cabochon stone. The setting is mounted on an easy to make split shoulder ring.
The lesson includes some great tips and tricks including an alternative way to set the stone in a thick bezel using a Whaley sliding hammer.
Lessons Include:
- Tigers Eye Ring - 54 mins 19 sec
Materials:
- 13mm x 18mm cabochon stone (round or different size can be used)
- Sterling silver strip 1.2mm x 3.3mm x 55mm & 1.5mm x 3.5mm x 55mm
- 0.7mm thick sheet 20mm x 25mm (approx)
- Author
You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.