How to Make a Stone Set Twist Wire Ring
- Description
This is a great lesson for jewelry students advancing their skills or creating a range of jewellery for sale.
One of the first techniques you will learn when making jewelry is 'how to make a twist ring'. This lesson shows you the easiest way.
You will then learn how to add a tube setting. The lesson includes instructions on how to make the setting as well as how to set the stone.
Lessons Include:
- Part 1 - Stone set twist wire ring - 33 min 56 sec
- Part 2 - Gold twist wire ring - 16 min 17 sec
- Part 3 - Chenier tube - 12 min 23 sec
- Plus PDF instructional download
Materials for stone set ring:
- 1.2mm x 180mm round wire
- Round faceted stone & a small section of tube with an outside diameter 1mm larger
- Includes
Purchase also includes these instructional PDF downloads:
- Makingcheniertube.pdf
- Author
You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.