How to Make Quick and Easy 3-Prong Claw Settings
- Description
This four claw setting technique can be used to mass produce small settings. You can the solder them onto your jewelry creation and stone set them to add bling and enhance its beauty.
This lesson includes two videos:
- Part 1 - Three claw settings - 29 min 38 sec
- Part 2 - How to make chenier tube - 12 min 23 sec
Materials:
- 3mm round faceted stones
- Tube with the same outside diameter
- 0.8mm round claw wire
- Includes
Purchase also includes these instructional PDF downloads:
- Makingchenier.pdf
- Author
You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.