How to Make a Knot Ring with a Set Stone
- Description
This is so simple to make and the end result looks great. You can make this knot ring without the stone or vary the shoulder opening. Great fun to make!
Lessons Include:
- Stone set knot ring - 26 min 34 sec
Materials:
- 3.75mm round stone
- Sterling silver round wire 140mm x 1.4mm
- Tube 4.5mm x 10mm (wall thickness approx 0.7mm)
- Author
You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.