How to Make Four Claw Oval Earrings
- Description
This lesson will guide you through the process of making a straight wall four claw setting to the stone dimensions. There is an excellent demonstration on fixing claws in one solder operation and can be applied to many projects. You will also learn how to make butterfly post backs.
Lessons included:
- Part 1 - Four claw oval earrings - 42 min 41 sec
- Part 2 - Butterfly clips - 13 min 27 sec
Materials:
- 2 x 9mm x 7mm oval CZ's
- Sterling silver strip; 0.8mm x 3.5mm x 120mm
- Sterling silver round wire; 0.9mm x 150mm
- Author
You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.