How to Make a 6-Claw Rex (Crown) Setting
- Length24 min 46 sec
- Description
This course will show you how to make a traditional rex setting that is stamped and formed from a disk. You will learn how to carve the prongs into it and size it to fit the stone you are working with.
Materials:
- Round stone size between 7mm - 7.5mm
- Sterling silver or other metal disk 1.2mm thick x 12.5m diameter or 2.3 grams scrap
- Author
You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.