How to Make a Four Claw Oval Pendant
- Description
This lesson will show you a simple way to make a straight-walled oval setting for a pendant. You will learn how to space the claws correctly, make a simple bail, and perform basic claw setting.
Lessons Include:
- Four claw oval pendant - 38 min 26 sec
Recommended materials: Sterling silver (or gold)
- 10mm x 12mm oval stone
- 0.8mm x 5mm x 55mm
- round wire; 0.8mm x 10mm
- round wire 1.2mm x 40mm
- Author
You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.