The Gem and Jewelry World's foremost Resource on The Internet.
Re: [Orchid] Kunzite fade in any light  
  [Thread Prev] [Message Prev]      [Date Index]   [Thread Index]      [Message Next] [Thread Next]
From: MarkH
Date: Thu Jul 03 22:12:56 2008
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========

Dear Leonid

>     Original post was about treatment of Kunzite with Cobalt 60.
>     In my response I did made a note that thr language would not be as
>     precise, as it would be required on a test. Somehow, it fell on
>     deaf ears. 

    Here are some of statements you made in the process of this thread.
    could you please verify them by true of false? 

>     Nickel 60 is high energy isotope in his own right and it does emit
>     Gamma (neutron) type radiation as a by-product of it's decay. 

    True or False? 

>     Nickel 60 is in exited state. It relaxes to lower energy state by
>     emitting excess of energy as a photon which is a gamma particle. 

    True or False? 

>     Photon is a Gamma particle and stream of Gamma particles is a
>     neutron radiation. 

    True or False? 

>     Neutron Radiation--is a term used to talk about energy being
>     released from atoms that have too much energy for one reason or
>     another. Radiation is in the form of energetic particles or
>     electromagnetic waves. 

    True or False? 

    What I am really after is a true/false explanation of your own words
    and not additional statements or explanations. 

Thanks
Marky
____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project