From: karen Date: Tue Feb 13 05:21:45 2007 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== You might want to investigate a small casting machine invented by Ti-Research. I see a lot of good products out on the market, but this casting machine is so good, I am working with a technical person in the US with McKinnon Global who will travel around the country and teach casting workshops at your studio. The whole set up is so easy and so small, it is perfect for the small studio jewelry designer. We are offering a three day workshop on Ti-Casting Machine at Metalwerx in May. The description hasn't been finalized, but the first two days will be working with wax and natural burnouts. The third day is open to the jewelry trade to watch live demonstrations in casting stainless and possibly platinum. I will be posting this up on my Metalwerx Insider in a few days and on Orchid. Meanwhile, go to http://www.mckinnon.global.com and take a look at the machine. -k Metalwerx ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project