========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== I have never used them the way you want but I have used a number of metal based anti sieze compounds copper based to about 1800 F . Hot times have been extended not days or hours. There are some nickel based ones that are rated to 2400 F. There are also some using mica for high temperatures. Many people sell these. Loc Tite is probably the easiest place to find some but any of the tool supply houses should carry somebodies. Another thing to try is using dissimilar metals for the nuts and bolts. I have always thought invar bolts might work better then the traditional ones. Used against steel or Stainless Steel plates you would increase the pressure on the work as the metal heated up. Using the anti sizes may take some experimentation. jesse ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project