From: Noel Yovovich Date: Tue Mar 09 23:11:48 2004 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi, Addy, My favorite way to solder chain into a tube to finish it off (which I do mostly with snake chain) is to insert the chain, allowing a bit of it to stick out the other side. I then solder it at that end, and trim/file off the excess. I lay a razor blade over the other end of the tube and chain to avoid having solder travel there or melting something. With a closed cap, I would put a piece of solder in first, then the chain, proceed as above, though of course there is no way to really know when you've done it other than quenching and pulling. Maybe someone else will give us both a tip on that. HTH! Noel ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project