    Vovin, welcome to wax injecting.  Don't knock the cheap little hand
    injector - it will do a good job for small shops, but you need to
    learn good techniques.  The wax sticking to the rubber means your
    wax temperature is way too high. Check the chart of the wax you use
    and, if necessary buy a special thermometer to make sure you stay in
    the range recommended by the manufacturer.   The raised letters
    vanishing sound like you are compressing the mold too tightly,
    squeezing off the expansion as the wax is forced in.  Relax your
    grip - or the mold holder clamp's.  That should solve your problem. 
    If it doesn't, slicing another small vent from that area could do
    the trick.  But look to your pressure first.  It all takes a bit of
    trial and error for a beginner.  Suggest you get a small notebook
    and record all settings for each mold and note where it works
    perfectly.  Relax and experiment, don't fight that machine, enjoy it.
    

Pat



____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project