brian Saturday, June 07, 2003
   
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========


    I use copper. A piece of 5mm wide strip and it digs out several rows
    of teeth at a time. The file cards I buy at our jewellery stores
    feature stainless steel wire that is actually too fat to fit into the
    teeth of the file. How could that work, I think. But the copper strip
    has been fab. 

Brian

-- 
B r i a n   A d a m   
B u s h  J e w e l l e r y  W o r k s h o p s
Auckland NEW ZEALAND
www.adam.co.nz/workshops/high_school/ high school jewellery





Click to Visit


Bookmark and Share Printer View Printer View
Navigate:
Orchid Resources:

 

Donate! If you believe in what we're doing, you can help!