The Gem and Jewelry World's Foremost Resource on The Internet. |
||||||||||
|
|||||||||||
Product Review: Stuller's Burnishing Compound MF610Stuller's high speed burnishing compound for magnetic finishers brightens jewelry and keeps magnetic pin media clean for best results By: Mark B. Mann Technical Contributions by Andy Kroungold, Tool Specialist, Stuller, Lafayette , LA Copyright © Mark Mann 2005 |
|||||||||||
After several years of use, the small stainless-steel pins in my magnetic finisher had became dark, were stuck together and yielding poor results when tumbling precious metal mountings. Seeking advice for improvement, I turned to Andy Kroungold, Stuller's tool specialist. He suggested using a modest amount of Stuller's concentrated liquid burnishing compound MF 610 at full strength for 1 hour in my magnetic finisher to clean the pins. The MF 610 transformed the dingy and off color pins back into a new and shiny condition. In addition, subsequent magnetic finishing procedures were vastly improved with shortened run times and brighter results on the pieces I was pre-finishing. Here's a quick overview of magnetic finishing and MF610:
|
|||||||||||
| All rights reserved internationally. Copyright © Mark Mann. Users have permission to download the information and share it as long as no money is made-no commercial use of this information is allowed without permission in writing from Mark Mann. | |||||||||||