[416] Gravers
Gravers are small cutting tools used for stone setting, texturing, de-burring and applying decorative embellishments and traditional hand engraving. Steps required to prepare new gravers include mounting, sizing, shaping, sharpening and proper storage. Gravers are among the most useful tools at a jeweler's bench. Failure to properly prepare and maintain gravers not only presents a hazard, but also affects quality of work, proper technique and time efficiency. Here are some steps for preparing gravers for utilization with hand techniques.... (2004)
Complete Story

Show me more articles from: [Visual Communications]|[Mark B. Mann]
Releated Categories:[Small Tools]|[Stone Setting]

 

[431] Hoover & Strong’s Tru-Seat Setting System
Hoover & Strong, Inc. in Richmond, VA provides a line of Tru-Seat settings that include solitaire earrings, pendants and solitaire rings in yellow, white and palladium white gold alloys. By using Tru-Seat mountings and the system outlined below, jewelers can reduce material costs, labor and improve quality..... (2004)
Complete Story

Show me more articles from: [Visual Communications]|[Mark B. Mann]
Releated Categories:[Small Tools]|[Stone Setting]

 

[370] Installing and Repairing Hinge Rivets Using Pulse-arc-Welding Technology
Installing or repairing hinge rivets can be difficult with a torch. Flooding a hinge with solder and permanently joining a link to adjacent links are among the risks when using a torch and solder. Use of the following pulse-arc welding techniques to weld the hinge rivets will eliminate potential problems and speed up the overall procedure..... (2004)
Complete Story

Show me more articles from: [Visual Communications]|[Mark B. Mann]
Releated Categories:[Hinges & Catches]|[Fusing & Welding]|[Repairs]

 

[813] Installing New Tapered Bezels Using Tack-Welding Technology
This ring is in for repair and reconstruction. When it was originally made, 6-prong settings were used to mount the customers diamonds. All prong tops are severely worn and one prong has broken. The customer has requested bezel settings, so the prong settings were removed from the ring. The ring was re-sized according to the customers request and then pre-finished. For tacking the tapered 14-karat yellow gold bezels, the brass tweezers lead was modified to firmly hold a bezel. A ball bur was used to remove metal from inside each end of the tweezers.... (2006)
Complete Story

Show me more articles from: [Visual Communications]|[Mark B. Mann]
Releated Categories:[Fusing & Welding]

 

[392] Jewelry Finishing Update Featuring Foredom's Bench Lathe Kit, Wheels and Accessories
Understanding and using updated materials will help you accomplish pre-finishing and finishing requirements professionally and efficiently. Here's a brief overview of some new and established products.... (2004)
Complete Story

Show me more articles from: [Visual Communications]|[Mark B. Mann]
Releated Categories:[Polishing]

 

Page 1 2 3 4 5 6 7 8 9 10  Next
 


 
Donate! If you believe in what we're doing, you can help!