The Gem and Jewelry World's Foremost Resource on The Internet.
 
   for   in     
Add Ganoksin Power Search to your website
 
| Site Map | Jewelry Making Articles | Orchid Forums & Archives | Members Blogs | Galleries | BenchTube - Jewelry Making Videos |
| The BenchExchange | MetalCalc | Industry Web Sites Guide | Featured Products | Advertising | Contact Us | Link to Us | RSS feeds| More...

  Tips from The jeweler's bench
The Gem and Jewelry World's foremost Resource on The Internet. Open to the public, Free of Charge!
We are here to build a strong pool of information for the benefit of Web's jewelers and craftsmen - and those interested in jewelry and gemstones.
 
     
 
 
 
 
 

Back
Excerpts from: Ganoksin
Page: 1 2 3 4 5 6 7 8 9 10  Next
 
[101] Morro Redondo Tourmaline
This is a report on the largest occurrence of Tourmaline in the history of Brazil gem mining; the Morro Redound Tourmaline of the State of Minas Gerias Brazil. The material was first discovered in 1992 near the village of Morro Redondo, in the northeast of Minas Gerias.... (1997)
Complete Story

Show me more articles from: [Ganoksin]|[Mark Liccini]
Releated Categories:[Gemstones Information]

 

[120] Nephrite and Jadeite
Two gemstones bear the name jade: nephrite and jadeite. Nephrite, first known as yu, was treasured by the Chinese for centuries. Its current name, and the word "jade," both came from the Europeans via the Spanish conquistadores who.... (2001)
Complete Story

Show me more articles from: [Ganoksin]|[Sandra I. Smith]
Releated Categories:[Gemstones Lore]

 

[85] Notes about Buffing and Polishing Materials
Almost any metal or hard plastic item can be buffed to a high polish or a satin sheen with the correct buffing wheel and the proper polishing compound. This includes copper pots, doorknobs, golf clubs and switch plates, to name a few common items. The molecular composition of different metals is as different as the appearance, density and luster of the metals themselves. To polish and enhance the shine on a beautiful piece of jewelry requires a totally different set of polishes and buffs than to get a real professional shine.... (2003)
Complete Story

Show me more articles from: [Ganoksin]|[John Fisher]
Releated Categories:[Polishing]|[Shop Machines]

 

[130] Opal - Water filled with fire
The fragile opal first flashed its fiery colors at mortals millennia ago, igniting a love affair that has survived the fickleness of the human heart. Its faults, like softness and lack of stability, are overlooked by those entranced by its beauty.... (2001)
Complete Story

Show me more articles from: [Ganoksin]|[Sandra I. Smith]
Releated Categories:[Gemstones Lore]

 

[463] Patinas - Formulas
The surface of metals may be colored, a patina added either chemically or with heat. Patinas are generally achieved by causing the metal present to react with another element. It may be the air forming oxides or another chemical added to bond molecularly with the surface. A few pseudo-patinas are simple coatings on the metal's surface. The following patina formulas are but a sampling of the hundreds in existence. The formulas selected illustrate the wide range of application methods employed as well as a rich variety of colors. The first 30 formulas listed are represented on a supplemental sampling chart to designed for use as a visualtext-book..... (2004)