The Gem and Jewelry World's Foremost Resource on The Internet.
 
   for   in     
Add Ganoksin Power Search to your website
 
| Site Map | Jewelry Making Articles | Orchid Forums & Archives | Members Blogs | Galleries | BenchTube - Jewelry Making Videos |
| The BenchExchange | MetalCalc | Industry Web Sites Guide | Press Room | Advertising | Contact Us | Link to Us | RSS feeds| More...

  Tips from The jeweler's bench
The Gem and Jewelry World's foremost Resource on The Internet. Open to the public, Free of Charge!
We are here to build a strong pool of information for the benefit of Web's jewelers and craftsmen - and those interested in jewelry and gemstones.
 
     
 
 
 
 
 

Back
Articles by Gregg Todd and Greg Gilman
Page:
 
[235] Five Steps for Successful Investing
A good practice for preventing investment blowout is to measure the height of the trees before investing. The maximum tree height should be between 0.5 inch and (for larger trees with more metal) 0.75 inch shorter than the fill level of the flask. It's also important to leave a 0.125 inch gap between the top of the investment and the top of the flask if you are using benchtop vacuum casting with a solid flask.... (2003)
Complete Story

Show me more articles from: [AJM]|[Gregg Todd and Greg Gilman]
Releated Categories:[Lost Wax Casting]|[Casting Troubleshooting]
ISBN: B00006K39S

 