An English excerpts from the book "Lost Wax Jewelry Making: The Build-up Technique" by Minoru Azama, printed in Japanese by Kashiwa Hobby Books. This article will guide you on the process of using the wax build-up techniques to create a ring shank and how to approach gemstone positioning and symmetry. You will also find information on how to create wax seats for soft porous minerals and stones. (2005) Complete Story
Aside from the visual pleasure one derives from a textured surface, the biggest benefit is the ease in finishing the cast piece. No filing, no burs, no abrasive points, and no scratch removal compounds are necessary. Simply use a wire brush on the flexshaft for a soft satin finish. If a mirror finish is desired, then go on to the polishing wheel.... (2005) Complete Story