[918] Japanese Chasing Tools
Japanese chasing tools are made from steel blanks available in Japan called tagane. Japanese chasing hammers are lightweight with long straight handles and smaller faces than European styles. They balance beautifully in the hand and are effortless to use. The type of Japanese chasing I learned was called uchidashi. Mostly a top-down technique, this style of chasing includes chiseling to remove material, line and dot inlay, and hammer engraving using a chisel. The tools are shaped at the working end to exact specifications including angles and millimeter measurements of the faces for their particular use.... (2009)
Complete Story

Show me more articles from: [Chasing & Repousse]|[Nancy Megan Corwin]
Releated Categories:[Chasing and repousse]|[Small Tools]
ISBN: 1929565321

 

Page
 


 
Donate! If you believe in what we're doing, you can help!