[117] Feldspar - Ubiquitous Mineral
Moonstone and sunstone, seemingly opposites because of their names, are in reality closely related members of the feldspar family. Formed when hot magma solidifies underground, feldspar makes up about 60% of the Earth's crust. It's found worldwide in one form or another. Mineralogists have identified at least 40 varieties of feldspar.... (2002)
Complete Story

Show me more articles from: [Ganoksin]|[Sandra I. Smith]
Releated Categories:[Gemstones Lore]

 

[255] Fine Silver Granulation - Part 1
Granulation is the process of fusing tiny metal spheres of silver or gold, in a decorative pattern, to a surface of the same metal. It is an ancient technique that produces a beautiful, delicate effect. When making Granulated jewelry, all connections are fused instead of soldered.... (2001)
Complete Story

Show me more articles from: [Ganoksin]|[Sandra Buchholz]
Releated Categories:[Granulation]

 

[256] Fine Silver Granulation - Part 2
Granulation involves placing and fusing tiny balls of silver on the surface of the backsheet in a preplanned design. The mixture of Hide Glue, flux and water is used to temporarily hold the granules in place until they are fused.... (2001)
Complete Story

Show me more articles from: [Ganoksin]|[Sandra Buchholz]
Releated Categories:[Granulation]

 

[472] Firescale Prevention During Vacuum Casting - An Inexpensive Method
Firescale has been the scourge of sterling silver casters since the first silver was poured into a mold. It has been a thorn in the side of silver fabricators. Fortunately there are ways to prevent fire scale while silver soldering. This paper describes a simple, inexpensive method of preventing fire scale during vacuum casting.... (2005)
Complete Story

Show me more articles from: [Ganoksin]|[Lee Epperson]
Releated Categories:[Casting]

 

[958] Free Full eBook: The Jewelry Maker
Full eBook.48 Pages: Jewelry and metalsmithing are hard work, and also very rewarding. There is great pleasure in creating with one´s hands, in the process of taking raw materials and creating something. It´s also fun to get dirty, and to bang really loud on a piece of metal. It´s wonderful to have someone say, "Gosh, I love your earrings," and being able to respond, "Thanks, I made them." So whatever brought you here, and whatever motivates you to stay, welcome, and let´s get to work! This book is a resource for you when you work on your own. The book is written as though you will be setting up your own workshop at home, so I discuss safety concerns, what type of tools to use, and how to set up your own area. Good luck and have a great time! (2007)
Complete Story

Show me more articles from: [Ganoksin]|[Elaine D. Luther]
Releated Categories:[Beginner's Corner]|[Selected Bibliography List]

 

Page 1 2 3 4 5 6 7 8 9 10  Next
 


 
Donate! If you believe in what we're doing, you can help!