The Gem and Jewelry World's Foremost Resource on The Internet.
 
   for   in     
Add Ganoksin Power Search to your website
 
| Site Map | Jewelry Making Articles | Orchid Forums & Archives | Galleries | The BenchExchange | MetalCalc |
| Industry Web Sites Guide | Press Room | Advertising | Contact Us | Link to Us | More...

  Tips from The jeweler's bench
The Gem and Jewelry World's foremost Resource on The Internet. Open to the public, Free of Charge!
We are here to build a strong pool of information for the benefit of Web's jewelers and craftsmen - and those interested in jewelry and gemstones.
 
     
 
 
Advertise Here!
 
 
 
 

Back
Articles by G. Raykhtsum
Page:
 
[304] Evaluation of strength and quality of chains
In recent years, we have witnessed a growing concern of manufacturers and retailers regarding the quality of the jewelry products. Closer attention is being paid to such issues as general aesthetic appearance, surface finish, color consistency, strength and overall durability of jewelry. Responding to the increasing quality requirements, we have made an attempt to develop some specific methods for testing the finished jewelry products including various chains, bangle bracelets, castings and components..... (1998)