The Gem and Jewelry World's Foremost Resource on The Internet.
 
   for   in     
Add Ganoksin Power Search to your website
 
| Site Map | Jewelry Making Articles | Orchid Forums & Archives | Galleries | The BenchExchange | MetalCalc |
| Industry Web Sites Guide | Press Room | Advertising | Contact Us | Link to Us | More...

  Tips from The jeweler's bench
The Gem and Jewelry World's foremost Resource on The Internet. Open to the public, Free of Charge!
We are here to build a strong pool of information for the benefit of Web's jewelers and craftsmen - and those interested in jewelry and gemstones.
 
     
 
 
 
 
 

Back
Excerpts from: Platinum Guild International
Page: 1 2 3 4 5 
 
[278] Maximizing Refining Returns for Platinum Alloys
Platinum jewelry manufacturing presents some very different concerns when discussing the collection of materials for refining purposes. The assumption that methods used for gold and silver collection and recovery can be used for platinum can lead to real problems and problems of perception.... (2003)
Complete Story

Show me more articles from: [Platinum Guild International]|[Robin White]
Releated Categories:[Refining]

 

[309] Platinum - Durability vs. Scratching
There is a major difference between durability and scratch resistance. Platinum is very durable. When scratched, the scratch actually displaces the metal, leaving ridges on the edges of the scratch. This is where durability comes in. Whereas other precious metals, if scratched, lose metal, and thus wear down, Platinum does so at a much slower rate.... (2002)
Complete Story

Show me more articles from: [Platinum Guild International]|[Jurgen J. Maerz]
Releated Categories:[Metals]|[Platinum Fabrication]|[Polishing]

 

[335] Platinum - Machines, Hands and Wedding Bands
If you have never manufactured with platinum and you think that you are ready, if you manufacture with platinum, but you have not capitalized on the growing potential of the bridal market, even if you are successful at manufacturing platinum bridal jewelry, I hope some of what is contained in this paper will be of help to you. I have been involved in wedding ring manufacturing for about 25 years. For the last eight years, I have committed a majority of my time to designing in platinum, and platinum and 18-karat gold combinations. I have always looked at my designing successes in our industry and equated them with my desire to explore. As a result of my last decade of studying, platinum and I have become great friends.... (1999)
Complete Story

Show me more articles from: [Platinum Guild International]|[Bruce Pucciarello]
Releated Categories:[Jewelry Mass Production]

 

[519] Platinum Alloy Applications for Jewelry
Today, platinum is enjoying its renaissance. In the U.S., platinum consumption has risen by more than 700% since 1990. More jewelers are carrying platinum jewelry, and consumers are becoming more aware of the most noble of all metals. Many jewelers are still confused as to the platinum alloys available, their application and purpose, this paper will attempt to clear up some of these issues.... (2000)
Complete Story

Show me more articles from: [Platinum Guild International]|[Jurgen J. Maerz]
Releated Categories:[Metallurgy]

 

[745] Platinum Alloys - Features and Benefits
In this presentation I attempted to provide you with information on platinum alloys to help you make an informed decision as to which alloy to employ for your manufacturing venture. There are several alloys I did not mention, mainly because they are experimental and have not found their way into the main stream. An alloy is chosen for its capability, ease of recycling and many other criteria. It must be user friendly, scratch and bend resistant and hold your stones securely. It is further of importance that it can be finished with few or no problems and hold a shine. These alloys that can do all this are here. They are on the market and can do just what you are looking for. It is sometimes just a matter of breaking old habits to see a major improvement in your product.... (2004)
Complete Story

Show me more articles from: [Platinum Guild International]|[Jurgen J. Maerz]
Releated Categories:[Metallurgy]

 