| [611] Champleve with Ferric Chloride |
Champleve (shahmp-luh-vay), meaning - raised plane - in French, is the process by which a design is cut, gouged or etched out of metal to create low areas for the enamel. After many layers of enamel have been fired, the piece is stoned and may be re-fired to restore a glossy finish. The unenameled metal areas may be waxed, polished or plated. I cut, clean and etch many pieces at one time, but I fire each piece separately. Each piece requires approximately 8 to 10 firings.... (2004)
 Complete Story |
| Show me more articles from: [Enameling with Professionals]|[Audrey Komrad] |
| Releated Categories:[Champleve] |
| ISBN: 0971925208 |
| [751] Cloisonne Beads of Fine Silver |
I have been making my cloisonne beads since 1996 in a variety of methods with fine silver and wires of fine silver or 24K gold for the designs. My method of fusing two domed halves of fine silver requires fewer metalsmithing skills than the other methods I use, which is why I have chosen to explain this one. Although I currently create my beads the way I describe here, the door is always open for experimentation....
(2004)
 Complete Story |
| Show me more articles from: [Enameling with Professionals]|[Linda Crawford] |
| Releated Categories:[Cloisonne Enamel] |
| ISBN: 0971925208 |
| [889] Cloisonne Jewelry with 24k Wires |
Merry-Lee Rae has been making jewelry since 1966 when she joined her father in the garage while he dabbled in metal arts. In 1976 she fell in love with enameling, and her life took a turn from hard-core academics to a relentless, obsessive pursuit of crafts. She feels privileged to have the support of her extraordinary family. She sees herself as a dedicated romantic. Her awards and achievements, the shows, the galleries, the private collections, and the lack of training are not as important to her as the people who arc touched by her work..... (2004)
 Complete Story |
| Show me more articles from: [Enameling with Professionals]|[Merry-Lee Rae] |
| Releated Categories:[Cloisonne Enamel] |
| ISBN: 0971925208 |
| [919] Cloisonne on Steel |
When Joseph Trippetti returned from the Army in 1946, he studied for three years at Philadelphia College of Art and the fourth year at Sheffield College of Arts and Crafts in England, where he majored in silversmithing. He has been enameling since the 1950s. For some years he taught enameling and painting before concentrating on commissions and gallery exhibitions. The medieval tapestries still influence his designs. His cloisonnes were on domed copper plaques before he turned to large steel tiles. (2004)
 Complete Story |
| Show me more articles from: [Enameling with Professionals]|[Joseph Trippeti] |
| Releated Categories:[Cloisonne Enamel] |
| ISBN: 0971925208 |
| [890] Enameling on Electroformed Vessels |
June Schwarcz (b.1918) in Denver, CO. She is a Fellow of the American Craft Council and received their Gold Medal. The museum collections that have her work include Metropolitan Museum, Renwick Gallery of the Smithsonian, and Kunstgewerbe Museum in Zurich, Switzerland. Mostly she makes electroformed, three-dimensional objects. The richness and brilliance of transparent enamels still fascinates her after 47 years of enameling.... (2004)
 Complete Story |
| Show me more articles from: [Enameling with Professionals]|[June Schwarcz] |
| Releated Categories:[3D Enameling] |
|
|
|
|
|
| |
| |