[736] Advanced Joining Techniques for Platinum Jewelry
Joining is a very important production technique in the field of jewelry production. Therefore it is useful to know, what kinds of different joining techniques are possible. This paper will give you a rough overlook on joining techniques as well as some tips and tricks to do a good joint between platinum and platinum, and between platinum and gold. Which technique to prefer depends on the worker skill and on the available equipment.... (2004)