We use a method for cutting down firescale when using a Presto-Lite Torch along with an acetylene B tank. The torch tips are engineered to take in so much gas through the gas orifice and so much air through the air inlet ventura so they burn to their max.... (1996) Complete Story
This project is for beginners that wish to become silversmiths, part time or full time. Keep in mind that there are many ways to do this faster with the use of mechanical tools, but you are doing this project to learn how to use your frame saw and how to solder... () (1996) Complete Story