on The Internet. Open to the public, Free of Charge! We are here to build a strong pool of
information for the benefit of Web's jewelers and craftsmen - and those
interested in jewelry and gemstones.
Champleve (shahmp-luh-vay), meaning - raised plane - in French, is the process by which a design is cut, gouged or etched out of metal to create low areas for the enamel. After many layers of enamel have been fired, the piece is stoned and may be re-fired to restore a glossy finish. The unenameled metal areas may be waxed, polished or plated. I cut, clean and etch many pieces at one time, but I fire each piece separately. Each piece requires approximately 8 to 10 firings.... (2004) Complete Story