[92] PLIQUE-A-JOUR - Russian Soldering Method
There are a number of methods for plique a jour, a filigree technique that allows light to shine through the enamel, much like stained glass. With plique a jour, there is no backing for the vitreous enamel; instead a structure of metal is made with open spaces, called cells, for the enamels. I form a framework of fine silver square wire and within that framework I solder wires.... (2003)