Interested in illuminating my work and using experimental techniques, I came across copper mesh. There are many kinds of mesh, but only a few are easily obtained without buying in bulk from industrial suppliers. I have been using the 'Impressions' mesh, from American Art Clay Co., with transparent enamels for making plique a jour pieces. The mesh can be purchased from a local craft store or online. There are three varieties available, ranging from dense cloth like mesh , to 1/8 to 1/4 inches diamond shaped expanded mesh.... (2002) Complete Story
Electroforming is the process of controlling the metal deposit from an anode metal, through electrolyte solution, onto an electroconductive surface. Basically, a skin of metal is built up into a rigid structure. The materials you will need to get started are as follows.... (2004) Complete Story