  Tips from The jeweler's bench
The Gem and Jewelry World's foremost Resource on The Internet. Open to the public, Free of Charge!
We are here to build a strong pool of information for the benefit of Web's jewelers and craftsmen - and those interested in jewelry and gemstones.
 
     
 
 
 
 
 

Back
Excerpts from: Brain Press Publications
Page: Previous  11 12 13 14 15 16 17 18 19 20  Next
 
[76] Small Scale Double Making Procedures
Double is a German word of french origin meaning rolled gold or gold fill material. I use it for the gold-fill material described here to differentiate it from the commercially produced sheet. Hand made double has different qualities than the manufactured metal. It is far less perfect, its finished size is limited by one's workshop facilities and counting hours it costs more per square centimeter.... (1985)
Complete Story

Show me more articles from: [Brain Press Publications]|[Charles Lewton-Brain]
Releated Categories:[Surface Manipulation]

 

[474] Solder Flow Retardant Notes
While goldsmiths normally strive to have their solder flow easily, there are times you don't want it to flow, such as spilling over a decorated surface, if it 'freezes' a mechanism, or if it threatens to open a gap in a seam soldered earlier in a construction. The best way of not melting earlier seams is.... (2004)
Complete Story

Show me more articles from: [Brain Press Publications]|[Charles Lewton-Brain]
Releated Categories:[Soldering]

 

[488] Soldering Many Parts at Once with a Pourable Soldering Jig
There is a great way of doing very complex and repeated solderings in one go. This very important method uses casting and soldering investment is to set up multiple solderings at once. The idea is that you take clay (I prefer real clay, not plasticine - less oil and grease present to impede soldering) and make a 'bed' of it, a slab. Some people like to use a soft wax like 'BonBell' wax that covers small round cheeses instead of clay.... (2005)
Complete Story

Show me more articles from: [Brain Press Publications]|[Charles Lewton-Brain]
Releated Categories:[Soldering]

 

[81] Some application methods for applying Patination solutions to metal surfaces
Extremely clean metal surfaces give better results. See the article on Cleaning metal Surfaces for more information on cleaning.... (1995)
Complete Story

Show me more articles from: [Brain Press Publications]|[Charles Lewton-Brain]
Releated Categories:[Patination]

 

[6] Some basic metal working tools for beginners
Making jewelry is sometimes seen as a difficult or an expensive proposition. In reality a basic metal working shop can be set up quite inexpensively. Cutting (separating materials), soldered construction and finishing are the three main things that jewellers do and what follows is a list of basic tools for doing these things. One should be able to set up a basic shop for less than a hundred dollars.... (1994)
Complete Story

Show me more articles from: [Brain Press Publications]|[Charles Lewton-Brain]