It is easy to forget that when we remove PMC from the kiln, what we have is a piece of metal and we can bring to bear on that piece any and all of the myriad techniques employed in regular metalworking.
With our standard PMC tools and not much more than an additional file, hammer, and a drill, we can incorporate other materials into our PMC and our PMC into other materials. I am using for this project Faux one, a PVC product that is easy to use, extraordinarily durable, inexpensive, and safe. It can be hammered, filed, sanded, polished, heated, molded, drilled, and carved. The PMC can be pushed around or into it and it is so tough you can hammer on it, which I do in the project presented here.... (2006) Complete Story