[142] Firing Created Moissanite and Diamonds into place in PMC
PMC is not a traditional material, and so a few pioneers went about tentatively setting cubic zirconia's, and lab grown corundum into the clay. For almost a decade it has been believed that natural stones would be destroyed in the sintering process. And so nobody took the risk. A few brave souls attempted to "cast" diamonds in place in the kiln. Proving to not only be a costly experiment, but.... (2002)