Invented in 1996 by Peter Johns, a professor of silversmithing at Englands Middlesex University, Argentium[R] Sterling Silver, like traditional sterling silver, is at least 92.5 percent pure silver. But unlike traditional sterling, which is 7.5 percent copper, Argentium sterling has a small amount of germanium instead of some of the copper. So how does that change things?.... (2006) Complete Story
With a simple corrugation tool and basic metalsmithing skills, you can make these great earrings. The newest toy in my studio is a Microfold Brake. I have been having a wonderful time learning what can be done with this tool, experimenting and making metalwork that combines microfolding with my other favorite techniques. I have used the Microfold Brake for bracelets, earrings, pins, boxes, a teapot, and a Hanukkah menorah, yet I feel like I am just getting started with my explorations! I find the immediacy of the tool very alluring. I also like the way the rippling corrugation can be either organic - or geometric looking, depending on how it is manipulated and
finished. (2003) Complete Story
Jeffrey Herman is an accomplished silversmith, master of holloware repair, and the founding director of the Society of American Silversmiths. His live/work space includes areas devoted to each of these specialties. The front door opens into a 25 by 40 foot open area that comprises living room, kitchen, drafting, and office spaces. The ceilings soar 13 feet above. Large windows frame a sunset view. The floors in this former brewery are marvelous old hardwood that has been polished and varnished, adding warmth, character, and a smooth surface for scooting around on a wheeled desk chair.... (2003) Complete Story