Firescale has been the scourge of sterling silver casters since the first silver was poured into a mold. It has been a thorn in the side of silver fabricators. Fortunately there are ways to prevent fire scale while silver soldering. This paper describes a simple, inexpensive method of preventing fire scale during vacuum casting.... (2005) Complete Story
This paper describes a process that eliminated fire scale during a vacuum casting cycle. Castings should not have a fire scale problem if the casting are cooled following this procedure....This casting was cooled using this process. This is what it looks like after quenching and brushing with a brass brush.... (2005) Complete Story
This paper describes two simple methods of creating a shield to be used on the end of a Foredom handpiece. The shield will prevent grindings and dust from being slung into the face. Always wear eye protection when using the handpiece.... (2005) Complete Story
This paper will describe how to turn a block of wax into a pottery of approximately 1 1/4 inches in diameter and 2 inches tall. The pottery was turned in two pieces. The lower section below the ring below the inlaid stones and the portion above the ring. I have turned wax that is 3 inches thick..... (2006) Complete Story