The Gem and Jewelry World's Foremost Resource on The Internet.
 
   for   in     
Add Ganoksin Power Search to your website
 
| Site Map | Jewelry Making Articles | Orchid Forums & Archives | Members Blogs | Galleries | BenchTube - Jewelry Making Videos |
| The BenchExchange | MetalCalc | Industry Web Sites Guide | Press Room | Advertising | Contact Us | Link to Us | RSS feeds| More...

  Tips from The jeweler's bench
The Gem and Jewelry World's foremost Resource on The Internet. Open to the public, Free of Charge!
We are here to build a strong pool of information for the benefit of Web's jewelers and craftsmen - and those interested in jewelry and gemstones.
 
     
 
 
 
 
 

Back
Excerpts from: Ganoksin
Page: 1 2 3 4 5 6 7 8 9 10  Next
 
[121] Diamond - Brilliant Ice
Currently identified with love, diamonds are the gemstone of choice in engagement, wedding, and anniversary rings. Contrary to popular belief, we have not always given diamonds as love tokens. That custom results from modern marketing techniques, not ancient traditions.... (2001)
Complete Story

Show me more articles from: [Ganoksin]|[Sandra I. Smith]
Releated Categories:[Gemstones Lore]

 

[117] Feldspar - Ubiquitous Mineral
Moonstone and sunstone, seemingly opposites because of their names, are in reality closely related members of the feldspar family. Formed when hot magma solidifies underground, feldspar makes up about 60% of the Earth's crust. It's found worldwide in one form or another. Mineralogists have identified at least 40 varieties of feldspar.... (2002)
Complete Story

Show me more articles from: [Ganoksin]|[Sandra I. Smith]
Releated Categories:[Gemstones Lore]

 

[255] Fine Silver Granulation - Part 1
Granulation is the process of fusing tiny metal spheres of silver or gold, in a decorative pattern, to a surface of the same metal. It is an ancient technique that produces a beautiful, delicate effect. When making Granulated jewelry, all connections are fused instead of soldered.... (2001)
Complete Story

Show me more articles from: [Ganoksin]|[Sandra Buchholz]
Releated Categories:[Granulation]

 

[256] Fine Silver Granulation - Part 2
Granulation involves placing and fusing tiny balls of silver on the surface of the backsheet in a preplanned design. The mixture of Hide Glue, flux and water is used to temporarily hold the granules in place until they are fused.... (2001)
Complete Story

Show me more articles from: [Ganoksin]|[Sandra Buchholz]
Releated Categories:[Granulation]

 

[472] Firescale Prevention During Vacuum Casting - An Inexpensive Method
Firescale has been the scourge of sterling silver casters since the first silver was poured into a mold. It has been a thorn in the side of silver fabricators. Fortunately there are ways to prevent fire scale while silver soldering. This paper describes a simple, inexpensive method of preventing fire scale during vacuum casting.... (2005)
Complete Story