The Gem and Jewelry World's Foremost Resource on The Internet.
 
   for   in     
Add Ganoksin Power Search to your website
 
| Site Map | Jewelry Making Articles | Orchid Forums & Archives | Members Blogs | Galleries | BenchTube - Jewelry Making Videos |
| The BenchExchange | MetalCalc | Industry Web Sites Guide | Press Room | Advertising | Contact Us | Link to Us | RSS feeds| More...

  Tips from The jeweler's bench
The Gem and Jewelry World's foremost Resource on The Internet. Open to the public, Free of Charge!
We are here to build a strong pool of information for the benefit of Web's jewelers and craftsmen - and those interested in jewelry and gemstones.
 
     
 
 
 
 
 

Back
Articles by Edna B. Anthony
Page: 1 2 3 4 
 
[284] Goshenite Beryl
Goshenite is the transparent, colorless, alkali-bearing pure beryl that was discovered in Goshen, Hampshire County, Massachusetts. The Lily Pond mine in a pegmatite near a small lake was the source of crystals accompanied by other pale greenish-blue, bluish-green, yellowish, pink, and white beryl crystals.... (1999)
Complete Story

Show me more articles from: [New Mexico Faceters Guild]|[Edna B. Anthony]
Releated Categories:[Gemstones Information]

 

[283] Green, Yellow-Green, and Brownish-Yellow-Green Beryls
Yellow-green beryl has achieved 'desired gem' status with consumers just within the last few years. Museums were eager to acquire spectacular specimens, while connoisseurs sought it for their collections. However, fashion trendsetters ignored it. As in aquamarine, the iron incorporated into its chemical structure is responsible for the color..... (1999)
Complete Story

Show me more articles from: [New Mexico Faceters Guild]|[Edna B. Anthony]
Releated Categories:[Gemstones Information]

 

[113] Kyanite - Polymorphic Aluminum Silicate Gem
Andalusite, kyanite, and sillimanite all contain identical amounts of aluminum, silicon, and oxygen, combined with other trace elements. I find it intriguing to note the differences in how the chemical formulas for these three minerals are expressed by many well-known authorities on gemstones. That list includes.... (2003)
Complete Story

Show me more articles from: [New Mexico Faceters Guild]|[Edna B. Anthony]
Releated Categories:[Gemstones Information]

 

[233] Let's talk Gemstones - Staurolite
Staurolite! Why would one of the most ordinary, patently unattractive minerals, used as a religious talisman and a good luck charm for centuries, be, in its transparent faceted form, a much sought after collector's gem? Rarity! Seldom do the dark reddish-brown or yellowish-brown transparent crystals occur in sufficiently light tones and sizes to warrant faceting.... ()
Complete Story

Show me more articles from: [New Mexico Faceters Guild]|[Edna B. Anthony]
Releated Categories:[Gemstones Information]

 

[271] Lets Talk Gemstones - Opal
Opal is a fascinating gemstone with an ancient history. Pliny the Elder gives an eloquent description of opal, comparing its many colors to that of the finest of ruby, emerald, sapphire, topaz, and amethyst. Romans prized opal so highly that one citizen of the highest rank suffered permanent exile for refusing to relinquish ownership of a magnificent hen-egg sized opal to the emperor..... (2000)