[267] Beginning Platinum
Platinum casting is different from gold or silver casting, and insufficient preparation and understanding of the process can still lead to many hours of frustration. Success depends on having good, functional equipment and process control, and learning all you can about the process before you cast your first flask.... (2003)
Complete Story

Show me more articles from: [Platinum Guild International]|[Jurgen J. Maerz]
Releated Categories:[Platinum Casting]

 

[293] Casting Gold to Platinum
The principle of bi-metal casting is really very simple: A wax model is invested, cast and finished. A secondary wax is created, which is going to become part of this piece. The wax is attached to the first casting, re-invested and the metal is cast on, thus creating a piece that is made with two metals. It is recommended that mechanical fastening devices, such as plugs, tracks etc. be worked into the design. The piece is then finished as usual.... (2003)
Complete Story

Show me more articles from: [Platinum Guild International]|[Jurgen J. Maerz]
Releated Categories:[Platinum Casting]

 

[824] Curve Ahead - Using Coils To Bend Tubing
Many tools sold in model/hobby stores can be used for jewelry making. During a recent visit to a hobby shop, I found these tube bending coils, which model makers use to build models that require bent tubing. Jewelry makers will find these coils handy when bending tubing for projects.... (2006)
Complete Story

Show me more articles from: [AJM]|[Jurgen J. Maerz]
Releated Categories:[Bench Tips & Tricks]
ISBN: B00006K39S

 

[792] Fabricating a Platinum Sphere Pendant with a Laser
It is becoming common practice to do more and more platinum fabrication with a laser welder. For this project, you need about a foot of 0.25 mm hard platinum wire. You can purchase hard wire from a metal supplier, or draw it down from a larger size without annealing to achieve the hardness required. You also need a wooden bead (the diameter of which is up to you), superglue, and a laser welder.... (2006)
Complete Story

Show me more articles from: [AJM]|[Jurgen J. Maerz]
Releated Categories:[Platinum Fabrication]|[Fusing & Welding]
ISBN: B00006K39S

 

[439] Fearless Platinum Repairs
What does it take to be successful at repairing, customizing, and servicing platinum jewelry? First, an understanding of properties unique to platinum. When platinum is mined, it is usually found with one or more of its five sister metals, called the platinum group metals: palladium, osmium, rhodium, ruthenium, and iridium.... (2003)
Complete Story

Show me more articles from: [Platinum Guild International]|[Jurgen J. Maerz]
Releated Categories:[Platinum Fabrication]|[Repairs]

 