If you benefit from what we're doing and want to give something in return, you can make a donation!
The Gem and Jewelry World's foremost Resource
on The Internet. Open to the public, Free of Charge! We are here to build a strong pool of
information for the benefit of Web's jewelers and craftsmen - and those
interested in jewelry and gemstones.
Standard yellow gold alloys which are based on gold-silver copper can be used for many production processes. They could be called ‘all-purpose’ alloys. However, optimising the alloys for the particular manufacturing process to be employed is possible by use of other alloying additions which can influence relevant properties such as castability and grain size as well as the mechanical ones, for example, strength, hardness and ductility. Only a few elements (e.g. zinc, silicon, iridium, cobalt) have proved to be useful additions for modifying carat gold alloys without detrimentally changing other relevant properties.... (2002) Complete Story