The Gem and Jewelry World's Foremost Resource on The Internet.
 
   for   in     
Add Ganoksin Power Search to your website
 
| Site Map | Jewelry Making Articles | Orchid Forums & Archives | Galleries | The BenchExchange | MetalCalc |
| Industry Web Sites Guide | Press Room | Advertising | Contact Us | Link to Us | More...

If you benefit from what we're doing and want to give something in return, you can make a donation!

  Tips from The jeweler's bench
The Gem and Jewelry World's foremost Resource on The Internet. Open to the public, Free of Charge!
We are here to build a strong pool of information for the benefit of Web's jewelers and craftsmen - and those interested in jewelry and gemstones.
 
     
 
 
Advertise Here!
 
 
 
 

Back
Articles by Fred Klotz
Page:
 
[351] Cold forging of karat gold findings
Cold forging in the karat gold jewelry industry has sometimes been referred to as stamping, coining and die striking. This process has been used throughout history in the making of coins and medals as well as jewelry. Cold forging basics will always be the same as they were during antiquity; however, the fine points are constantly being refined. The process is simply described as forming a finding by using extreme force to drive raw material into a shaped cavity in a steel block. While it may sound simple, there are many subtle conditions that will effect the outcome.... (2002)
Complete Story

Show me more articles from: [The World Gold Council]|[Fred Klotz]
Releated Categories:[Die Forming]

 

[410] Live And Let Die (Struck)
In a manufacturing environment, there are numerous pitfalls and problems that will conspire to prevent successful completion of a job. Some of these problems may be complex and involve highly technical investigations, explanations and resolutions; however, many are basic, avoidable mistakes that are easily remedied.... (2002)
Complete Story

Show me more articles from: [The World Gold Council]|[Fred Klotz]