The Gem and Jewelry World's Foremost Resource on The Internet.
 
   for   in     
Add Ganoksin Power Search to your website
 
| Site Map | Jewelry Making Articles | Orchid Forums & Archives | Galleries | The BenchExchange | MetalCalc |
| Industry Web Sites Guide | Press Room | Advertising | Contact Us | Link to Us | More...

  Tips from The jeweler's bench
The Gem and Jewelry World's foremost Resource on The Internet. Open to the public, Free of Charge!
We are here to build a strong pool of information for the benefit of Web's jewelers and craftsmen - and those interested in jewelry and gemstones.
 
     
 
 
Advertise Here!
 
 
 
 

Back
Articles by Sandra Noble Goss
Page:
 
[318] Advanced Etching of Copper, Brass and bronze
This method of etching uses a prepared ferric chloride solution which also contains hydrochloric acid. This 'etchant' is not a pure acid, but etches copper and copper alloys (like brass and bronze). It will not work on silver. It is available from electronics supply shops, such as Radio Shack or from chemical suppliers. It is generally used to clean or etch copper circuit boards. It can also be found at some printmakers' supply stores.... (2004)
Complete Story

Show me more articles from: [MetalWerx]|[Sandra Noble Goss]
Releated Categories:[Etching]

 

[319] Multi-Metal Lamination - aka Metal Overlay
Multi-metal Lamination is a type of 'faux' married metal which produces a freer, more 'painterly' effect than the hard-edge, highly graphic, married metal. It is a technique in which designs may appear to float over other shapes and patterns. MML may be used in a figurative way or to produce over-all pattern. MML is achieved by layering patterns of different coloured metals on top of a thick base plate. The patterns are soldered onto the surface, and then compressed by passing through a rolling mill. The resulting illusion is of a single piece of metal with patterns of different coloured metals 'inlaid' into the surface..... (2004)
Complete Story

Show me more articles from: [MetalWerx]|[Sandra Noble Goss]