This method of etching uses a prepared ferric chloride solution which also contains hydrochloric acid. This 'etchant' is not a pure acid, but etches copper and copper alloys (like brass and bronze). It will not work on silver. It is available from electronics supply shops, such as Radio Shack or from chemical suppliers. It is generally used to clean or etch copper circuit boards. It can also be found at some printmakers' supply stores.... (2004) Complete Story
Multi-metal Lamination is a type of 'faux' married metal which produces a freer, more 'painterly' effect than the hard-edge, highly graphic, married metal. It is a technique in which designs may appear to float over other shapes and patterns. MML may be used in a figurative way or to produce over-all pattern. MML is achieved by layering patterns of different coloured metals on top of a thick base plate. The patterns are soldered onto the surface, and then compressed by passing through a rolling mill. The resulting illusion is of a single piece of metal with patterns of different coloured metals 'inlaid' into the surface..... (2004) Complete Story