[888] Casting Notes for Silver Lost Wax Casting
Casting of silver can be fairly easy and these notes are the results of my experience through trial and error as well as instruction from an experienced jeweler and instructor. Mark Ruby the instructor for the Fort Collins Senior Center was instrumental in helping with these notes and instructions. The person that has helped me test and experiment with the different methods is Mary Jo Ziedler. We have made some mistakes and we have had our successes. Mary Jo and I have only performed investment and casting using centrifugal equipment.... (2009)
Complete Story

Show me more articles from: [Ganoksin]|[Ken Moore]
Releated Categories:[Lost Wax Casting]

 

Page
 


 
Donate! If you believe in what we're doing, you can help!