| [666] Enameling Safety Issues |
Enameling involves the firing and melting of suitable glasses onto and into metals for decorative effects. It is done at fairly high temperatures, from 1200F (649C) to a high kiln temperature of 1700F (927C) or so.The primary dangers involve dusts, the particle size of the enamel used, the chemical constituents of the enamel (older enamels frequently contain lead and other toxic metal oxides and chemicals), the infrared radiation of the kiln and sundry opportunities to burn oneself. Enamelists in factories have even been killed by scalds from water when molten enamel was dumped into it.... (1999)
 Complete Story |
| Show me more articles from: [The Jewelry Workshop Safety Report]|[Charles Lewton-Brain] |
| Releated Categories:[Workshop Safety]|[Enameling] |
| ISBN: 0969851049 |
| [173] Gas handling |
Jewelers work with compressed gases of all kinds, in torch systems, kilns, casting machines, abrasive blasters, laser welding machines needing argon and more. Many of these gases are flammable and an explosion hazard, acetylene, propane and hydrogen are examples. Oxygen is often used with these gases. Oxygen is a potent fire risk if it comes in contact with oils, greases or flammable materials, even fingerprint grease left in a fitting has caused a fire before.... (1999)
 Complete Story |
| Show me more articles from: [The Jewelry Workshop Safety Report]|[Charles Lewton-Brain] |
| Releated Categories:[Workshop Safety] |
| ISBN: 0969851049 |
| [174] Grinding Wheel Safety Thoughts |
Besides the safety instructions that you get from a tool manufacturer in the tool manual it may be necessary for you to write your own sets of rules up to keep you out of trouble. This is especially important with employees. What follows is an example of thinking about what can go wrong with a tool. The tool used as an example is a mounted grinder. You can do the same sort of rule compilation with all the tools in your shop. See the "General Safety Rules for Tools" article as a starting point, then each tool will have certain idiosyncrasies which need to be noted. Think of it as "What advice would I give to someone to keep them out ot trouble on this machine?".... (1998)
 Complete Story |
| Show me more articles from: [The Jewelry Workshop Safety Report]|[Charles Lewton-Brain] |
| Releated Categories:[Workshop Safety]|[Shop Machines] |
| ISBN: 0969851049 |
| [931] Hammering and Forging Safety Notes |
Goldsmiths and silversmiths use hammers frequently in their work, silversmiths especially. A regular trade goldsmith might use a bench hammer with a ring on a mandrel twenty or more times a day. Blacksmithing operations use coal fires, gas torches and kilns..... (1998)
 Complete Story |
| Show me more articles from: [The Jewelry Workshop Safety Report]|[Charles Lewton-Brain] |
| Releated Categories:[Workshop Safety] |
| ISBN: 0969851049 |
| [229] Have your studio separate from your home |
Often craftspeople start out making craft objects in their living space, a kitchen, a living room, and sometimes continue working in them even when they have grown to the point that they need a separate studio. It is not wise to share one's living and family space with workshop space. Usually there are chemicals, tools, equipment, processes, sounds, materials, wastes, dusts and so on that are unhealthy to be exposed to that are produced in a work shop.... (2000)
 Complete Story |
| Show me more articles from: [The Jewelry Workshop Safety Report]|[Charles Lewton-Brain] |
| Releated Categories:[Workshop Safety]|[Beginner's Corner]|[Critical Notes] |
| ISBN: 0969851049 |
|
|
|
|
| |
| |