When burnishing very detailed pieces, use stainless pins in your mixed shot. Don’t use them any other time because the pins will often strike the work pieces with the pointed ends, creating a very undesirable pitting or orange peel appearance. If you must try mixing pins with your other stainless steel media, the pins can be removed with a medium strength magnet. I use the kind of magnet.... (2003) Complete Story