The Gem and Jewelry World's Foremost Resource on The Internet.
 
   for   in     
Add Ganoksin Power Search to your website
 
| Site Map | Jewelry Making Articles | Orchid Forums & Archives | Members Blogs | Galleries | BenchTube - Jewelry Making Videos |
| The BenchExchange | MetalCalc | Industry Web Sites Guide | Press Room | Advertising | Contact Us | Link to Us | RSS feeds| More...

  Tips from The jeweler's bench
The Gem and Jewelry World's foremost Resource on The Internet. Open to the public, Free of Charge!
We are here to build a strong pool of information for the benefit of Web's jewelers and craftsmen - and those interested in jewelry and gemstones.
 
     
 
 
 
 
 

Back
Articles by Mark B. Mann
Page: Previous  11 12 13 14 15 16 17 18 19 20 
 
[812] Setting & Shank Assembly Using Tack-Welding Technology
Setting and shank assemblies are routine work in many retail manufacturing jewelry shops. Heres a method for expediting this process using ABI tack-welding technology.... (2006)
Complete Story

Show me more articles from: [Visual Communications]|[Mark B. Mann]
Releated Categories:[Fusing & Welding]

 

[373] Shortening Bracelet Using Pulse-arc-Welding Techniques
This Charles and Colvard created moissanite (hereafter referred to as moissanite) and two-tone karat gold in-line bracelet requires shortening by two links. The bracelet is held together by a heavy link-wire that's wrapped around an open portion of the adjacent link and permanently joined, giving the bracelet maximum flexibility. Below is a procedure for shortening, reassembling and permanent welding of the link using pulse-arc-welding technology..... (2004)
Complete Story

Show me more articles from: [Visual Communications]|[Mark B. Mann]
Releated Categories:[Fusing & Welding]|[Repairs]

 

[374] Sizing a Platinum Ring Using Pulse-arc Welding Technology
Sizing and torch welding a platinum ring with diamonds channel set down the shank could be risky to the diamonds. Use of a Pulse-arc Welder for this welding job will eliminate the risk and potential damage.... (2004)
Complete Story

Show me more articles from: [Visual Communications]|[Mark B. Mann]
Releated Categories:[Fusing & Welding]|[Repairs]

 

[423] The 3M Radial Bristle Disc Proficiency Advantage
3M Radial Bristle Discs were introduced to the jewelry industry in 2000. Additional discs and end brushes have been added to the selection and over time and with the extensive selection I've reinvented how I semi-finish castings and perform other pre-finishing techniques. They are flexible, cool running, clean, non-loading and provide a controllable uniform finish. Here's an overview of semi-finishing a rough casting using the discs.... (2004)
Complete Story

Show me more articles from: [Visual Communications]|[Mark B. Mann]
Releated Categories:[Small Tools]

 

[530] The creation of AGTA 2004 Spectrum Award Winning Cufflinks by Bill Holman
These cufflinks designed by Bill Holman were award winners in the AGTA 2004 Spectrum design competition. They are 18-karat yellow gold and feature Drusy agates with a 24-karat deposition layer over the exposed crystal formation. The small gemstones are 1.50 millimeter diamond-cut round sapphires. In this article, Holman shares the details of his approach for making these award-winning cufflinks and how.... (2005)
Complete Story

Show me more articles from: [Visual Communications]|[Mark B. Mann]
Releated Categories:[Fabrication]|[Behind The Design]

 

Page Previous  11 12 13 14 15 16 17 18 19 20