[86] Iridescent Patina
This is the basic recipe for the iridescent patina. This patina is most effective on highly textured pieces, such as torch texture, rollerprinted and reticulation. It has a slight color interference pattern, similar to oil on water. It has a high natural luster, similar to the nacre on pearls, if done correctly with many repeated dips in a weak solution. It is durable, the colors remain stable to a high degree, and.... (2003)
Complete Story

Show me more articles from: [Ganoksin]|[Katherine Palochak]
Releated Categories:[Patination]

 